Nimonic 80A Studs Nimonic 80A studs is a metal rod or bar with threads on both sides. It also known as double-headed screws or studs, used to connect two parts together. General for mining machinery, bridges, cars, motorcycles, boiler steel structure, hanging tower, large span steel structure...

    Nimonic 80A Studs
    Nimonic 80A studs is a metal rod or bar with threads on both sides. It also known as double-headed screws or studs, used to connect two parts together. General for mining machinery, bridges, cars, motorcycles, boiler steel structure, hanging tower, large span steel structure and large buildings. 

    We tend to use studs when the parts need to remove frequently, because the thread will be worn if install and remove often, then we need to change the studs.

    Nimonic 80A is a nickel-based superalloy composed of Ni-Cr. In the high temperature with good strength and very excellent corrosion resistance and oxidation resistance. These advantages make the Nimonic 80A widely used in aerospace, aerospace, power stations and transportation and other high temperature hot forging parts.
    Nimonic 80A Chemaical composition:

    Alloy

    %

    Ni

    Cr

    Fe

    Mn

    Si

    P

    S

    Al

    Ti

    C

    Co

    B

    Zr

    Cu

    625

    Min.

    Balance

    18






    1.0

    1.8






    Max.


    21

    3.0

    1.0

    1.0

    0.02

    0.015

    1.8

    2.7

    0.1

    2.0

    0.008

    0.15

    0.2

    Nimonic 80A Physical properties:

    Density

    8.19 g/cm3

    Melting range

    1320-1365℃

    Nimonic 80A minimum mechanical properties in the room temperature:

    Status

    Tensile strength
      Rm N/mm2

    Yield strength RP0.2N/mm2

    Elongation A5 %

    Nimonic 80A

    930

    620

    20